About Fe-based Amorphous

About Fe-based Amorphous

The fe-based amorphous ribbon is made by applying molten steel to a finished thin ribbon by quick cooling solidification methods. Compared with traditional metal magnetic materials, the amorphous alloy is high in magnetoconductivity (10 times more than that of ferrite) and low in loss (1/5~1/10 that of silicon steel and 1/2~1/5 ferrite) due to the disordered arrangement of its atoms. It is an excellent soft magnetic material, which can take the place of silicon steel, permalloy or ferrite to be a transformer core, mutual inductor, sensor, and so on. With a Fe-based amorphous strip, the efficiency of the transformer will be improved and its size, weight, and energy consumption kept low.

The Fe-based amorphous strip is known as dual energy-saving material because it is made by environmentally-friendly processes and used in environmentally-friendly products:

1. Energy-saving manufacturing processes: Compared with traditional metallurgical processes (silicon), rapid solidification technology eliminates the need for complex machining processes, reducing energy consumption by about 80%. Statistically, the production of one kilogram of amorphous alloy strip saves one liter of oil compared to the production of 1 kg of cold-rolled silicon steel sheet;

2. Energy-saving products: At present, the Fe-based amorphous materials have been successfully used in electrical and electronic transformers. The transformer load loss is reduced by more than 70%, and the amorphous distribution transformer with the capacity of 315kVA saves 5000 kW/h annually, reducing carbon dioxide emissions by 4.5 tons.

Properties of Fe-based amorphous alloy compared to cold-rolled silicon steel sheets


Performance Indicators Fe-based amorphous alloy Cold rolled silicon steel
Saturation magnetic induction (T) 1.56 2.03
Coercivity (A/m) ≤4 ≤30
Maximum permeability <20xl04 4xl04
Iron loss 50 Hz 1.35T(W/kg) <2 <0.8
Exciting power 50Hz 1.35T(VA/kg) <0.4 <0.95
Lamination factor >0.85 0.96
Magnetostrictive coefficient 27xl06
Resistivity μΩ.cm 130 0.45
Density (g/cm3) 72 7.65
Crystallization temperature (℃ ) 550
Layer temperature (℃ ) 415 746
Tensile strength ( MPa ) 1500-2000 343
Vickers hardness ( HV) 900 181
Thickness (μm ) 30 300

Works

E-42 (B1, B2, C1) RIICO Industrial Area, Khushkhera-301707, District: Alwar, Rajasthan.
+91-11-26289502/03

www.advancedamorphous.com

info@advancedamorphous.com

Regd. Off.

1202, Ansal Tower, 38, Nehru Place, New Delhi-110019
+91-8810388842

www.advancedamorphous.com

info@advancedamorphous.com



Get In Touch

Follow Our Activity

Interactively coordinate proactive e-commerce via process-centric “outside the box“ thinking.